Polymer Property : Middle Barrel Temperature = 466 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 241 - 254 °C
466 - 489 °F
Injection Molding
Ineos ABS Lustran® 433 ABS, General-Purpose Injection Molding Grade
Lustran® ABS 433 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It is a high-impact, high-gloss ABS, available only in natural (000000) and black (904000)...
Middle Barrel Temperature 241 - 254 °C
466 - 489 °F
Injection Molding
Ineos ABS Lustran® 633 ABS, Injection Molding Grade
Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical ..