Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/920 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified
(discontinued **) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/960 Polyolefin, Unspecified
(Unverified Data**) Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without .. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CAT 10 Polyolefin Catalyst CAT 10 is a high density based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst CT 0552/09 Polyolefin Catalyst CT 0552/09 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst LV/1 Polyolefin Catalyst LV/1 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 Black Polyolefin Catalyst PS/2 is a PE based black catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2 UV Polyolefin Catalyst PS/2 UV is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LR Polyolefin Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or .. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/2LRO Polyolefin Catalyst PS/2LR0 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Catalyst PS/4 Polyolefin Catalyst PS/4 is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or st.. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Cogegum® AFR/920-UV Polyolefin Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: st.. |
|||
Zone 2 | 150 - 165 °C | 302 - 329 °F | |
Solvay Specialty Polymers Cogegum® GFR/320 Polyolefin Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly.. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Polidan® EC/110 Polyethylene, Crosslinked (XLPE) Polidan® XLPE-PEX -Cross-linkable Polyethylene. Low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be use.. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE) Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com.. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Polidan® EC/MD Polyethylene, Crosslinked (XLPE) Medium density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards complying.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0553/23 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0553/23 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® PNT 0856/35 Polyethylene, Crosslinked (XLPE) POLIDAN® PNT 0856/35 is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction.Features: Crosslinkable; Good Flexibility; Lo.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A Polyethylene, Crosslinked (XLPE) POLIDAN® T/A is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Features.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LV Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LV is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-LX Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-LX is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 2 | 150 - 200 °C | 302 - 392 °F | |
Solvay Specialty Polymers Polidan® T/A-SP Polyethylene, Crosslinked (XLPE) POLIDAN® T/A-SP is a silane crosslinkable PE compound which is used together with a catalyst masterbatch to accelerate the crosslinking reaction. It is used for flexible crosslinkable pipes.Featu.. |
|||
Zone 2 | 150 - 170 °C | 302 - 338 °F | |
Solvay Specialty Polymers Polidiemme® G/420 Thermoset Elastomer (TSE) Polidiemme® XLPO -Cross-linkable Polyolefin. Elastomer based compound crosslinkable by ambient moisture, consisting of a silane pregrafted base compound to be used with a catalyst masterbatch (Si.. |
|||
Zone 2 | 150 °C | 302 °F | |
Borealis Visico™ LE0540 Polyethylene Semiconductive Compound, Crosslinkable Visico™ LE0540 is a silane crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Visico™ LE0540 is highly suitable for co-extrusion with LDP.. |
|||
Zone 2 | 150 °C | 302 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D828 Ethylene Acrylate Appeel® 20D828 is an modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad temp.. |
|||
Zone 2 | 150 °C | 302 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D867 Ethylene Acrylate DuPont™ Appeel 20D867 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Zone 2 | 150 °C | 302 °F | Blown Film Coextrusion |
DuPont™ Appeel® 22D843 Ethylene Acrylate DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable .. |
|||
Zone 2 | 150 °C | 302 °F | Blown Film Coextrusion |
DuPont™ Appeel® 72D727 Sealing Resin DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP.. |
|||
Zone 2 | 150 °C | 302 °F | Blown Film Coextrusion |
DuPont™ Appeel® 20D784 Ethylene Acrylate Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature .. |