Material Notes:
Flame Retardant; Good UV Resistance; Halogen Free; Low Smoke Emission; Low Toxicity; Self ExtinguishingUses: Cable Jacketing; Low Voltage Insulation; Wire & Cable ApplicationsExtrusion equipment: standard extruders for thermoplastics equipped with low compression screw (1:1.2-1.4 compression ratio and 20-25 L/D ratio are suggested), and an adequate barrel thermoregulation.Additional Properties: Bending Test - IEC 60811 (-25°C): Pass; Calorific Potential - ISO 1716 18.0 MJ/kg; Cold Impact - IEC 60811 (-25°C): Pass; Collar Temperature - 170 to 180 °C; Corrosive Gas in Smoke - IEC 60754-2 < 10.0 µS/mm; Corrosive Gas in Smoke - IEC 60754-2 > 4.30; Halogenidric Acid Emissions - IEC 60754-1 < 0.10 %; Head Temperature - 180 to 190 °C; Heat Shock - IEC 60811 (150°C): Pass; Hot Pressure Test - IEC 60811 (90°C): < 50 %; Insulation Resistance Constant - IEC 60502 (20°C): 3000 Mohm·km; Insulation Resistance Constant - IEC 60502 (70°C): 200 Mohm·km; Temperature Index (Burning) - NES 715 280 °C; Water Absorption - IEC 60811 (100°C): 1.00 mg/cm²Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 1000 hour

@Thickness 3.00 mm,
Temperature 50.0 °C
>= 1000 hour

@Thickness 0.118 in,
Temperature 122 °F
Condition A, Compression Molded, 10% Igepal; ASTM D1693
Melt Flow 18 g/10 min

@Load 21.6 kg,
Temperature 190 °C
18 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
ISO 868
Tensile Strength at Break 14.5 MPa
2100 psi
ASTM D638
Elongation at Break 190 %
190 %
ASTM D638
Thermal Properties Metric English Comments
Oxygen Index 37 %
37 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+13 ohm-cm

@Temperature 70.0 °C
5.40e+13 ohm-cm

@Temperature 158 °F
ASTM D257
8.10e+14 ohm-cm

@Temperature 20.0 °C
8.10e+14 ohm-cm

@Temperature 68.0 °F
ASTM D257
Processing Properties Metric English Comments
Zone 1 130 - 150 °C
266 - 302 °F
Zone 2 150 - 170 °C
302 - 338 °F
Zone 3 160 - 180 °C
320 - 356 °F
Zone 4 170 - 180 °C
338 - 356 °F
Die Cooling Temperature 180 - 200 °C
356 - 392 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
RoHS Compliance RoHS Compliant