Polymer Property : Zone 2 = 165 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Zone 2 155 - 165 °C
311 - 329 °F
Lubrizol Advanced Materials Pearlbond® 12F75UV Thermoplastic Polyurethane
Pearlbondâ„¢ 12F75UV is a UV-resistant standard polyester-based TPU supplied in form of translucent, colorless pellets, featuring a low melting point and very low gel content. Processed by extrus..
Zone 2 155 - 165 °C
311 - 329 °F
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer
PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten..
Zone 2 150 - 165 °C
302 - 329 °F
Solvay Specialty Polymers Cogegum® GFR/320 Polyolefin
Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound. Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a poly..