Material Notes:
Catalyst PS/2LR is a PE based catalyst masterbatch, which accelerates the crosslinking reaction of the pipe product during its curing process that can take place by exposure of the pipe to water or steam at high temperature. Catalyst PS/2LR contains a processing aid and a lower reactive agent which in certain conditions improves processingFeatures: Antioxidant; Good Thermal Aging ResistanceUses: Piping; Plumbing Parts; Potable Water ApplicationsAdditional Properties: Extruder Screw Compression Ratio - >2.5:1; Extruder Screw L/D Ratio - 25:1 to 30:1; Head Temperature - 200 °CInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Apparent Bulk Density 0.550 g/cc
0.0199 lb/in³
ASTM D1895
Melt Flow 0.50 g/10 min
0.50 g/10 min
ISO 1133
Processing Properties Metric English Comments
Zone 1 150 - 200 °C
302 - 392 °F
Zone 2 150 - 200 °C
302 - 392 °F
Zone 3 150 - 200 °C
302 - 392 °F
Zone 4 150 - 200 °C
302 - 392 °F
Zone 5 150 - 200 °C
302 - 392 °F
Die Cooling Temperature 210 °C
410 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Processing Technique Extrusion; Pipe Extrusion