Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 210 - 230 °C | 410 - 446 °F | |
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers.. |
|||
Zone 1 | 190 - 230 °C | 374 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1047D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 1 | 210 - 230 °C | 410 - 446 °F | |
Lehmann & Voss LUVOCOM® 100-7126 VP Thermoplastic polyurethane, with PTFE Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K.. |
|||
Zone 1 | 220 - 230 °C | 428 - 446 °F | |
Eurostar Staramide P1000IX1 PA6, Impact Modified, Injection Molded Staramide P1000IX1 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI006 or Star X 2006)Information provided by Eurostar. |
|||
Zone 1 | 220 - 230 °C | 428 - 446 °F | |
Eurostar Staramide P1000IX2 PA6, Impact Modified, Injection Molded Staramide P1000IX2 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI010 or Star X 2010)Information provided by Eurostar. |
|||
Zone 1 | 220 - 230 °C | 428 - 446 °F | |
Eurostar Staramide P1000IX3 PA6, Impact Modified, Injection Molded Staramide P1000IX3 is an Impact Modified, Polyamide 6 Injection Molding Resin (also known as P1000HI020 or Star X 2020)Information provided by Eurostar. |
|||
Zone 1 | 220 - 230 °C | 428 - 446 °F | |
Eurostar Staramide P1000J5 PA6, Impact Modified, Injection Molded Staramide P1000J5 is a Low Temperature Impact Modified, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 220 - 230 °C | 428 - 446 °F | |
Eurostar Starpylen M1000-BK1A987 PP, Carbon Black Starpylen M1000-BK1A987 is a high carbon black load PP resinInformation provided by Eurostar. |
|||
Zone 1 | 220 - 230 °C | 428 - 446 °F | Extrusion Molding |
LG Chemical KEYFLEX BT S5035 Ester Type TPE Description: Injection Molding, TPC-ET, Airbag Cover Deployment, Medium Modulus, Black ColorApplication: Airbag Cover (DAB, PAB, KAB, SAB)CAS: 37282-12-5, 24968-12-5 and 1333-86-4Information provide.. |