Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excellent hydrolysis and microbial resistance. It can be both extruded and injection-molded.PEARLTHANE® 16N95UV when extruded, can be used for making (pneumatic) tubes, profiles and cables. When processed by injection molding, can be used for technical parts.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
ASTM D2240
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D412
Elongation at Break 575 %
575 %
ASTM D412
100% Modulus 0.0110 GPa
1.60 ksi
ASTM D412
300% Modulus 0.0160 GPa
2.32 ksi
ASTM D412
Tear Strength 130 kN/m
742 pli
ASTM D624 (Die C)
Abrasion 40
40
loss (mm³); DIN 53.516
Compression Set 30 %

@Temperature 23.0 °C,
Time 252000 sec
30 %

@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395B
44 %

@Temperature 70.0 °C,
Time 86400 sec
44 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395B
Thermal Properties Metric English Comments
Melting Point 178 - 188 °C
352 - 370 °F
MQSA 111
Glass Transition Temp, Tg -31.1 °C
-24.0 °F
DSC, 50°F/10min; ISO 11357-2
Processing Properties Metric English Comments
Feed Temperature 200 °C
392 °F
Nozzle Temperature 210 °C
410 °F
Zone 1 180 - 195 °C
356 - 383 °F
Zone 2 190 - 210 °C
374 - 410 °F
Zone 3 200 - 220 °C
392 - 428 °F
Zone 4 190 - 210 °C
374 - 410 °F
Die Temperature 185 - 195 °C
365 - 383 °F
Mold Temperature 35.0 °C
95.0 °F
Moisture Content <= 0.10 %
<= 0.10 %
MQSA 44
Screw Speed 50 rpm
50 rpm