Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Premix Thermoplastics Inc.
Trade Name PRE-ELEC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Premix Thermoplastics PRE-ELEC® ESD 4400 Static Dissipative Thermoplastic Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PRE-ELEC® ESD 4400 is a static dissipative thermoplastic compound based on PE-LD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 4400 has been developed for multilayer film blowing. It can also be injection moulded. Surface resistance values of 109 ohms (EOS/ESD S11.11-1993, IEC 61340-5-1) can be achieved with optimum processing parameters.Applications: Multilayer bags and sacks which give permanent ESD protection for the electronics, medical, pharmaceutical and agricultural industries. PRE-ELEC ® ESD 4400 gives also good printability without treatment and can be coloured into various bright colours. Processing: PRE-ELEC ® ESD 4400 compound can be processed on conventional PE-LD and PE-LLD blown film extrusion lines.Information from Premix OY
Physical Properties Metric English Comments
Density 0.980 g/cc
0.0354 lb/in³
Thickness 30.0 - 50.0 microns
1.18 - 1.97 mil
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 30.0 MPa
4350 psi
ISO 527
Film Tensile Strength at Yield, TD 18.0 MPa
2610 psi
ISO 527
Film Elongation at Break, MD 520 %
520 %
ISO 527
Film Elongation at Break, TD 475 %
475 %
ISO 527
Film Elongation at Yield, MD 520 %
520 %
ISO 527
Film Elongation at Yield, TD 320 %
320 %
ISO 527
Film Tensile Strength at Break, MD 30.0 MPa
4350 psi
ISO 527
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ISO 527
Electrical Properties Metric English Comments
Surface Resistance <= 1.00e+11 ohm
<= 1.00e+11 ohm
ISO IEC 61340-5-1
Static Decay <= 2.0 sec
<= 2.0 sec
ISO IEC 61340-5-1
Processing Properties Metric English Comments
Zone 1 180 - 200 °C
356 - 392 °F
Extruder
200 - 225 °C
392 - 437 °F
Die
Zone 2 185 - 205 °C
365 - 401 °F
Extruder
200 - 225 °C
392 - 437 °F
Die
Zone 3 190 - 210 °C
374 - 410 °F
Extruder
200 - 225 °C
392 - 437 °F
Die
Zone 4 195 - 215 °C
383 - 419 °F
Extruder
200 - 225 °C
392 - 437 °F
Die
Zone 5 200 - 220 °C
392 - 428 °F
Extruder
200 - 225 °C
392 - 437 °F
Die
Blow-up Ratio (BUR) >= 1.5
>= 1.5
Drying Temperature 60.0 °C
140 °F
Dry Time 3 hour
3 hour
Shelf Life 12.0 Month
12.0 Month
Normal Storing Conditions
Copyright © lookpolymers.com All Rights Reserved