Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Die Temperature = 190 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Die Temperature 180 - 190 °C
356 - 374 °F
Extrusion
ExxonMobil Dytron™ XK7300-92 Thermoplastic Elastomer  (discontinued **)
A hard, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is flexible and halogen-free, and is intended mainly for extrusion of ca..
Die Temperature 160 - 190 °C
320 - 374 °F
Extrusion Blow Molding
LG Chemical LUTENE-H BE0400 HDPE
Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con..
Die Temperature 185 - 190 °C
365 - 374 °F
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU
PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT..
Die Temperature 175 - 190 °C
347 - 374 °F
Borealis BS2581 High Density Polyethylene for Blow Molding
BS2581 is a high density polyethylene intended for blow molding products with high stiffness and very good environmental stress crack resistance (ESCR). Applications: industrial chemicals, househol..
Die Temperature 175 - 190 °C
347 - 374 °F
Borealis Bormed™ HD850MO Polypropylene Copolymer for Healthcare Applications
Bormed HD850MO is a medium melt flow rate polypropylene homo polymer using the Borealis Nucleation Technology (BNT). This provides a polypropylene with excellent dimensional stability and its high c..
Die Temperature 175 - 190 °C
347 - 374 °F
Borealis Borstar® BB2581 HDPE for Blow Molding
Borstar BB2581 is a high-density polyethylene intended for blow molding of products with high stiffness and very good environmental stress crack resistance (ESCR).Borstar BB2581 is recommended for h..
Die Temperature 175 - 190 °C
347 - 374 °F
Borealis BS2541 High Density Polyethylene
BS2541 is a high density polyethylene with very high ESCR This product is intended for blow molding. Applications: household and chemical containers such as detergents, cleaners, and motor oils, an..
Die Temperature 150 - 190 °C
302 - 374 °F
Hotmelt Coating Slot Die
EMS-Griltech Griltex® D 1531E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Die Temperature 185 - 190 °C
365 - 374 °F
Equate EMDA-6200 HDPE Blow Molding Resin
EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for ..
Copyright © lookpolymers.com All Rights Reserved