Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Estane® ALR CL87A Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type: Estane® ALR CL87A is an aliphatic, polycaprolactone-based TPU with a Shore A Durometer of 85-90.Features: Contains a UV package that enhances outdoor weatherability. This high performance resin is clear, UV resistant, it will not discolor and has excellent mechanical properties.Uses: Outdoor applications, protective films and graphics.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation Provided by The Lubrizol Corporation
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
ASTM D792
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 175 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 347 °F
ASTM D1230
Mechanical Properties Metric English Comments
Hardness, Shore A 85 - 90

@Time 5.00 sec
85 - 90

@Time 0.00139 hour
ASTM D2240
Tensile Strength, Ultimate 62.16 MPa
9015 psi
ASTM D412
Elongation at Break 410 %
410 %
ASTM D412
100% Modulus 0.00689 GPa
1.00 ksi
ASTM D412
300% Modulus 0.0157 GPa
2.28 ksi
ASTM D412
Flexural Modulus 0.0214 GPa
3.10 ksi
ASTM D790
Processing Properties Metric English Comments
Zone 1 165 °C
329 °F
Extrusion
Zone 2 170 °C
338 °F
Extrusion
Zone 3 175 °C
347 °F
Extrusion
Zone 4 180 °C
356 °F
Extrusion
Die Temperature 180 °C
356 °F
Extrusion
Melt Temperature 180 °C
356 °F
Extrusion
Users viewing this material also viewed the following: