Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 20 min | 20 min | Working Time |
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,.. |
|||
Pot Life | 20 - 25 min | 20 - 25 min | Mass: 50g; TM R050-19 |
Resinlab® EP1340 Medium Viscosity, Flame Retardant Epoxy Casting Resin System Resinlab™ EP1340 is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034) for U.. |
|||
Pot Life | 20 min | 20 min | |
Huntsman HY 356 Aliphatic Amine Mix Ratio with GY 6010 is 35.Comments/Applications: A medium viscosity phenol free aliphatic amine adduct. Industrial maintenance, coatings, tank lining, pipe coatings and flooring.Data provided b.. |
|||
Pot Life | 20 - 25 min | 20 - 25 min | |
Fibre Glast 1099 Room Temperature Epoxy Surface Coat Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that c.. |
|||
Pot Life | 20 - 22 min | 20 - 22 min | Time before parts must be mated |
Lord Adhesives 206 Long Working Time Acrylic Adhesive Lord 200 SeriesLord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range f.. |
|||
Pot Life | 20 - 30 min | 20 - 30 min | Time before parts must be mated |
Lord Adhesives 370 Two Component Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 20 - 45 min | 20 - 45 min | Time before parts must be mated |
Lord Adhesives 410 Flexible, High Impact and Peel Resistance, Long Working Time Acrylic Adhesive Lord 400 SeriesLord 400 Series Acrylic Adhesives offer extremely high impact and peel strength. The bond minimally prepared metals and plastics, and achieve high shear strengths. They also provide e.. |
|||
Pot Life | 20 - 30 min | 20 - 30 min | Time before parts must be mated |
Lord Adhesives 521 Medium Viscosity, Slow Cure Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Pot Life | 20 - 40 min | 20 - 40 min | Time before parts must be mated |
Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic Adhesive Lord Adhesives 660 White, Non Sag, Fast Set for FRP Acrylic AdhesiveLord 660 Acrylic Adhesive bonds FRP (fiber-reinforced plastics) with minimal surface preparation. Lord 660 can cross-bond FRP to m.. |
|||
Pot Life | 20 min @Temperature 25.0 °C |
20 min @Temperature 77.0 °F |
Based on 100 gram mass |
Lord Adhesives Thermosetâ„¢ UR-340 Two Component Urethane Encapsulant Lord UR-340 is a two component, room temperature curing, urethane encapsulating compound. It is low in viscosity and has excellent flow characteristics. Its flexibility, low modulus characteristics,.. |
|||
Pot Life | 20 - 30 min | 20 - 30 min | |
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable .. |
|||
Pot Life | 20 - 35 min | 20 - 35 min | 100 gram batch |
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
Pot Life | 20 - 30 min | 20 - 30 min | 100 gram batch |
Master Bond EP41S-1HTND Non-Drip, High Performance Epoxy Adhesive Description: Master Bond EP41S-1HTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a 100 to 30 mix ratio by weight and its viscosity is a smooth pas.. |
|||
Pot Life | 20 min | 20 min | 100 grams |
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Pot Life | 20 min | 20 min | |
Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive TRA-BOND 2122 is a versatile aluminum metal filled epoxy formulation developed for modern industrial casting, bonding and repair applications where a strong aluminum-like adhesive is required. This .. |
|||
Pot Life | 20 min @Temperature 25.0 °C |
20 min @Temperature 77.0 °F |
|
Trelleborg Emerson & Cuming EP574 Adhesive Clear unfilled adhesive for thin bond lines.All information provided by Trelleborg Emerson & Cuming |
|||
Pot Life | 20 min | 20 min | |
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c.. |
|||
Pot Life | 20 min | 20 min | 2 grams |
Tra-Con Tra-Bond F109CLR Fiber Optic Epoxy Adhesive TRA-BOND F109CLR is a clear, low viscosity epoxy specially designed for terminating plastic fibers. This blush free epoxy is an excellent choice for high humidity environments where absolute clarity.. |
|||
Pot Life | 20 min | 20 min | |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Pot Life | 20 min | 20 min | |
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy Product Description: EPO-TEK® 509FM-1 is a two component, optically opaque epoxy designed for potting of semiconductors, PCB and systems-level electronics. It can be used in many electronic indust.. |
|||
Pot Life | 20 min | 20 min | |
Abatron AboWeld 8104-13 Polysulfide-Epoxy Sealant and Caulk AboWeld 8104-13 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It has high hardness and rigidity, very low elongation, and is often used with sand or o.. |
|||
Pot Life | 20 min | 20 min | |
Abatron WoodEpox® Wood Replacement Compound WoodEpox® is a shrink-free adhesive putty wood replacement compound that can be used in any thickness in structural and decorative applications to replace, repair, extend, or fill wood and material.. |
|||
Pot Life | <= 20 min | <= 20 min | |
Aremco Ceramacast™ 900 High Temperature Potting & Casting Material Zirconia Silicate High Density, high strength molding compound. |
|||
Pot Life | 20 - 30 min | 20 - 30 min | |
Abatron AboCast 22-30/AboCure 50-12 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo.. |
|||
Pot Life | 20 min @Temperature 25.0 °C |
20 min @Temperature 77.0 °F |
200 g |
Abatron AboCast 8110-2/AboCure 8110-3 Flexible Epoxy This epoxy system can achieve flexibility and plasticity without sacrificing adhesive, electrical, structural, and other properties. This compound is a clear (unfilled) basic formulation. Its applic.. |
|||
Pot Life | 20 min | 20 min | |
Tra-Con Tra-Bond 2130 Medium Viscosity Epoxy Adhesive TRA-BOND 2130 is a clear, near transparent, medium viscosity epoxy adhesive formulation developed for rigid laminating, sealing and bonding applications where the combination of good wetting plus im.. |
|||
Pot Life | 20 min | 20 min | Mass: 50g; TM R050-19 |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |
|||
Pot Life | 20 - 30 min | 20 - 30 min | Mass: 100g; TM R050-19 |
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro.. |