Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Abatron AboCast 22-30/AboCure 50-12 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Cast, Unreinforced
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 22-30/AboCure 50-12 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/AboCure 50-12 is a fast, thick, hard, tough, filled, black, opaque, room-temperature-cure, lower-viscosity epoxy system. It offers high chemical and heat resistance, ceramic-like hardness, faster hardening and faster curing. AboCure 50-12, however, requires a precise ratio. The system is used for encapsulation, potting, and assembly of electronic and magnetic components, such as: capacitors, transformers, terminals, industrial magnets, small and large magnetic assemblies, metal detectors, metal separators, magnetic printing cylinders, magnetic holders, insulators, junction boxes, switches, and circuit boards. It is also used in general-purpose casting and bonding for structural and dielectric applications.
Physical Properties Metric English Comments
Density 0.983 g/cc
0.0355 lb/in³
AboCure 50-12
1.49 g/cc
0.0537 lb/in³
AboCast 22-30
Water Absorption 0.25 %

@Time 605000 sec
0.25 %

@Time 168 hour
Viscosity 9500 cP
9500 cP
Mechanical Properties Metric English Comments
Compressive Strength 118 MPa
17100 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 °C
239 °F
Deflection Temp at unknown load
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
"A"
Processing Properties Metric English Comments
Pot Life 20 - 30 min
20 - 30 min
Descriptive Properties Value Comments
Color Black
Parts by Weight (pbw) 100
AboCast 22-30
6
AboCure 50-12
Copyright © lookpolymers.com All Rights Reserved