Polymer Property : Pot Life = 30 min Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Pot Life 20 - 30 min
20 - 30 min
Resin Technology Group 120-EX Oxy-Bond™ Two-Component Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Pot Life 20 - 30 min
20 - 30 min
Resin Technology Group 120-EX Oxy-Bond™ Two-Component Epoxy Adhesive
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma..
Pot Life 20 - 30 min
20 - 30 min
Small Mass(15gr.)
Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive
Mix ratio 2 to 1 by volume.TIGA 202-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 202-EX offers a 20 minute pot life and good hardness development within..
Pot Life 25 - 30 min
25 - 30 min
ASTM D2471
Fibre Glast 1100 Light-Weight High-Strength Patching/Filler Compound
Product Features:Very Light Weight MaterialNon-Hazardous Product - Safe to UseEasily Sanded and Carved with Shop ToolsNegligible ShrinkageNon-Critical, 2 to 1 Ratio by Weight or by VolumeExcellent N..
Pot Life 20 - 30 min
20 - 30 min
Time before parts must be mated
Lord Adhesives 370 Two Component Epoxy Adhesive
Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh..
Pot Life 20 - 30 min
20 - 30 min
Time before parts must be mated
Lord Adhesives 521 Medium Viscosity, Slow Cure Acrylic Adhesive
Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi..
Pot Life 20 - 30 min
20 - 30 min
Time before parts must be mated
Lord Adhesives 7500B Two-Component, 100% Solids Urethane Adhesive
Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe..
Pot Life 15 - 30 min
15 - 30 min
Time before parts must be mated
Lord Adhesives 7542D Two-Component Urethane Adhesive
Lord Urethane AdhesivesLord® one- and two-part urethane adhesives provide superior bonds with minimal surface preparation for today's high performance thermosets and thermoplastics. They offe..
Pot Life 20 - 30 min
20 - 30 min
Master Bond EP38 Low Viscosity, Fast Curing, Two Component Epoxy
Master Bond Polymer System EP38 is a fast curing, low viscosity, optically clear two component epoxy system for high performance coating, bonding and sealing. EP38 has a unique balance of favorable ..
Pot Life 20 - 30 min
20 - 30 min
100 gram batch
Master Bond EP41S-1HTND Non-Drip, High Performance Epoxy Adhesive
Description: Master Bond EP41S-1HTND is a two component epoxy resin system for high performance bonding, sealing and coating. It has a 100 to 30 mix ratio by weight and its viscosity is a smooth pas..
Pot Life 25 - 30 min
25 - 30 min
200 gram mass
Master Bond Supreme 11AO Electrically Isolating Adhesive and Sealant
Description: Master Bond Polymer System SURPEME 11AO is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevated..
Pot Life 20 - 30 min
20 - 30 min
Abatron AboCast 22-30/AboCure 50-12 Epoxy
AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo..
Pot Life 25 - 30 min

@Temperature 24.0 °C
25 - 30 min

@Temperature 75.2 °F
1/2 lb mass
BCC Products BC 5008-2 General Purpose Epoxy System
BC 5008-2 is a very low viscosity, modified, unfilled, room temperature curing, general purpose resin system. BC 5008-2 is a clear, amber, medium pot life material, with heat resistance to 175ºF. A..
Pot Life 15 - 30 min

@Temperature 24.0 °C
15 - 30 min

@Temperature 75.2 °F
BCC Products BC 84 PVA Parting
BC 84 PVA Parting/Green is a water/alcohol solution of water soluble, film forming materials. It is particularly recommended as a parting layer for separation between polyester or epoxy resins and v..
Pot Life 25 - 30 min

@Temperature 24.0 °C
25 - 30 min

@Temperature 75.2 °F
1 lb. mass
BCC Products BC 5010 Epoxy Laminating System
BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor..
Pot Life 20 - 30 min
20 - 30 min
Mass: 100g; TM R050-19
Resinlab® EP1240RC Flame Retardant Epoxy Casting Resin
Resinlab™ EP1240RC is a medium viscosity, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File# E186034, Pro..
Pot Life 15 - 30 min
15 - 30 min
Mass: 50g; TM R050-19
Resinlab® EP1310 Medium Reactivity Epoxy Encapsulant
Resinlab™ EP1310 is a two part medium reactivity epoxy encapsulant capable of being quickly gelled prior to full cure by exposing to a UV light source. Usually 5- 10 seconds is sufficient to gel th..