Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 2122 Metal Repair Aluminum Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 2122 is a versatile aluminum metal filled epoxy formulation developed for modern industrial casting, bonding and repair applications where a strong aluminum-like adhesive is required. This two-part 100% reactive epoxy system is easy to use as it bonds readily to aluminum and other non-ferrous and ferrous materials, to wood, ceramics, glass, concrete and to many plastics. It has low shrinkage, and cures fairly rapidly to a hard, tough solid. Fully cured TRA-BOND 2122 is strong and durable, and is further resistant to mild acids and alkalis, water, salts and salt solutions, petroleum solvents, lubricating oils, gasoline, jet fuels, alcohol and many other organic and inorganic compounds. It is a non-magnetic electrical insulator, does not rust, and can be drilled, sawed, cut and machined with regular metal working tools. TYPICAL REPAIR APPLICATIONS: molds, dies, fixtures, plumbing, automotive castings, aircraft, marine, salvage, ships, jigs, tool repair, small part manufacturing. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 60000 cP

@Temperature 25.0 °C
60000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Adhesive Bond Strength 9.65 MPa
1400 psi
Lap shear, alum to alum, 24 hrs @ 25°C
23.4 MPa
3400 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Shrinkage 0.15 %
0.15 %
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
Dielectric Constant 8.5

@Frequency 1000 Hz
8.5

@Frequency 1000 Hz
Dielectric Strength 3.94 kV/mm
100 kV/in
Dissipation Factor 0.10

@Frequency 1000 Hz
0.10

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 20 min
20 min
Descriptive Properties Value Comments
Color Aluminum
Mix Ratio, parts by weight 100/18
Resin/Hardener