Material Notes:
AboWeld 8104-13 is a 2-part, 100% solids, liquid or filled polysulfide-epoxy. It is available in many colors. It has high hardness and rigidity, very low elongation, and is often used with sand or other fillers and pigments for patching, bonding, filling holes, etc. It is mainly used as a resurfacing coating, adhesive, and filler.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Tensile Strength at Break 19.0 MPa
2750 psi
Elongation at Break 25 - 30 %
25 - 30 %
Processing Properties Metric English Comments
Cure Time 1440 - 4320 min
24.0 - 72.0 hour
(1-3 Days)
Pot Life 20 min
20 min
Descriptive Properties Value Comments
Color Many Colors
Parts by Weight (pbw) 1
Part A
1
Part B
Users viewing this material also viewed the following: