Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Glass Bead Filled , Polypropylene with 10% Glass Fiber Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to themodification. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
Linear Mold Shrinkage, Transverse 0.014 cm/cm
0.014 in/in
Melt Flow 10 g/10 min

@Load 0.325 kg,
Temperature 270 °C
10 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 2.25 GPa
326 ksi
Flexural Strength 51.0 MPa
7400 psi
Flexural Modulus 2.18 GPa
316 ksi
Charpy Impact Unnotched 2.50 J/cm²

@Temperature -20.0 °C
11.9 ft-lb/in²

@Temperature -4.00 °F
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.500 J/cm²

@Temperature -20.0 °C
2.38 ft-lb/in²

@Temperature -4.00 °F
0.600 J/cm²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
Vicat Softening Point 156 °C
313 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2 hour
2 hour
Moisture Content <= 0.20 %
<= 0.20 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi