Material Notes:
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safety use /hockey, building/, protection frames of cardoors. Withstands high dynamic stress up to - 40°C. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Viscosity Measurement 2.3 - 2.8
2.3 - 2.8
Melt Flow 2.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
2.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
Tensile Modulus 2.07 GPa
300 ksi
Flexural Modulus 0.0700 GPa
10.2 ksi
Charpy Impact Unnotched 4.40 J/cm²

@Temperature -20.0 °C
20.9 ft-lb/in²

@Temperature -4.00 °F
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Charpy Impact, Notched 1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
5.90 J/cm²

@Temperature -20.0 °C
28.1 ft-lb/in²

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
Glow Wire Test 650 °C
1200 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 33.0 kV/mm
838 kV/in
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi