Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVAMID 66 BT Polyamide 66

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 66 BT Polyamide 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at low temperatures. Use in automotive, electrical, engineering and consumer goods industry. Application: electric tools, gear wheels, clamps, fasteners, toolbodies, webbing slings for cable harnesses.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0193 cm/cm
0.0193 in/in
STN 64 0808
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 80.0 MPa
11600 psi
STN EN ISO 527-2
Elongation at Break 3.0 %
3.0 %
STN EN ISO 527-2
Tensile Modulus 3.20 GPa
464 ksi
STN EN ISO 527-2
Flexural Strength 110 MPa
16000 psi
STN EN ISO 178
Flexural Modulus 2.70 GPa
392 ksi
STN EN ISO 178
Charpy Impact Unnotched 9.00 J/cm²

@Temperature -20.0 °C
42.8 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
10.0 J/cm²

@Temperature 23.0 °C
47.6 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.150 J/cm²

@Temperature -20.0 °C
0.714 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.200 J/cm²

@Temperature 23.0 °C
0.952 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
STN EN ISO 75/A
Vicat Softening Point 250 °C
482 °F
B; STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
STN IEC 60093
Dielectric Strength 30.0 kV/mm
762 kV/in
STN IEC 60243
Comparative Tracking Index 600 V
600 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 960
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi