Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin
(discontinued **) Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 - 221 °C | 399 - 430 °F | |
Chevron Phillips mPact™ D449 HDPE Blown Film Resin
(discontinued **) Resin Type: High density, hexene copolymerCharacteristics: excellent clarity, high gloss, good modulus, process with LLDPE setup, optimum clarity when used as an individual layer.Applications: overw.. |
|||
Processing Temperature | 204 - 274 °C | 399 - 525 °F | Average value: 238 °C Grade Count:10 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 710 Utility Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 720 Black ABS Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | Injection |
Shuman 790 Black and Custom Colors ABS-Flame Retardant Excellent flame retardancy, good impact strength, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 810 Black Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 811 Black Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 880 Grey Polystyrene High Impact Good impact strength, injection molding and extrusion grades, easy processability, good surface appearance, good gloss.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 227 °C | 399 - 441 °F | |
Shuman 881 Grey Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Processing Temperature | 204 - 310 °C | 399 - 590 °F | Extrusion |
Dyna-Purge® C Purging Compound Designed for Purging Transparent ResinsGeneral Description:DYNA-PURGE C is a clear, non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to purge high clarity.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109 LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109DJ LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 7109M LLDPE Blown Film Resin Resin Type: linear low density polyethylene, hexene copolymerCharacteristics: good stiffness at thin gauges, good drawdown, excellent processability, can use straight or in blends with LDPE or HDPE,.. |
|||
Processing Temperature | 204 °C | 399 °F | |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |
|||
Processing Temperature | 204 - 246 °C | 399 - 475 °F | Typical |
ExxonMobil PP7032E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good Colorabilit.. |
|||
Processing Temperature | 204 - 246 °C | 399 - 475 °F | Typical |
ExxonMobil PP7033E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate.Availability: North America and Asia Pacific Featu.. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7035E4 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7035E5 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow DOWLEX™ 2032 Linear Low Density Polyethylene, Blown Film Grade DOWLEX® 2032 Polyethylene resin is a general purpose liner resin having improved thermal stability over a broad range of processing conditions. It is an outstanding choice for thin gauge, medium st.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 526A Low Density Polyethylene, Blown Film Grade DOW LDPE 526A resin is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains medium levels of antiblock additive. .. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Processing Temperature | 204 - 232 °C | 399 - 450 °F | Typical |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 493A Low Density Polyethylene, Film Grade DOW LDPE 493A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 493A resin can be blended with most linear low density.. |
|||
Processing Temperature | 204 °C | 399 °F | Film extrusion temperature |
Dow LDPE 494A Low Density Polyethylene, Film Grade DOW LDPE 494A resin, is a high strength, general purpose resin used for shipping sack, industrial liner and produce film applications. DOW LDPE 494A resin can be blended with most linear low density.. |
|||
Processing Temperature | 204 - 260 °C | 399 - 500 °F | Stock Temperature |
Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Processing Temperature | 204 - 221 °C | 399 - 430 °F | Optimum Extrusion Temperature |
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer