Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 204 - 246 °C | 399 - 475 °F | Typical |
ExxonMobil PP7032E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection-molding, extrusion and thermoforming applications.Availability: North America Features:Good Colorabilit.. |
|||
Processing Temperature | 204 - 246 °C | 399 - 475 °F | Typical |
ExxonMobil PP7033E2 Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate.Availability: North America and Asia Pacific Featu.. |