Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Meets FDA Regulation 177.1520.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D1505
Melt Flow 6.5 g/10 min
6.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
ASTM D790
Electrical Properties Metric English Comments
Dielectric Constant 2.33

@Frequency 100000 Hz
2.33

@Frequency 100000 Hz
ASTM D1531
Dielectric Strength 20.0 kV/mm

@Thickness 3.17 mm
508 kV/in

@Thickness 0.125 in
ASTM D149
Dissipation Factor >= 0.00010

@Frequency 100000 Hz
>= 0.00010

@Frequency 100000 Hz
ASTM D1531
Processing Properties Metric English Comments
Processing Temperature 204 - 260 °C
399 - 500 °F
Stock Temperature