Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shuman 720 Black ABS

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Shuman
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 720 Black ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good impact strength, easy processability, good chemical resistance, good wear and abrasion resistance.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Izod Impact, Notched 2.14 J/cm
4.01 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.0 °C
169 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 177 - 216 °C
351 - 421 °F
Extrusion
204 - 227 °C
399 - 441 °F
Injection
Users viewing this material also viewed the following: