ExxonMobil PP7033E2 Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil PP7033E2 Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: A high crystallinity, high impact copolymer resin designed for injection molding applications requiring medium melt flow rate.Availability: North America and Asia Pacific Features:Good ColorablityGood Dimensional StabilityMedium FlowMedium Impact ResistanceUses: Automotive ApplicationsAutomotive Interior PartsAutomotive Interior TrimChild Safety SeatsConsumer ApplicationsToysProcessing Method: Injection MoldingAutomotive Specifications: Hyundai MS213-24 Type 6 Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.8 MPa
3600 psi
2 in/min; ASTM D638
Elongation at Yield 6.4 %
6.4 %
2 in/min; ASTM D638
Flexural Modulus 1.12 GPa
163 ksi
1% secant, 0.05 in/min.; ASTM D790
1.30 GPa
189 ksi
1% secant, 0.5 in/min; ASTM D790B
Izod Impact, Notched 2.30 J/cm
4.30 ft-lb/in
ASTM D256
Gardner Impact 23.8 J

@Thickness 3.17 mm,
Temperature -30.0 °C
17.6 ft-lb

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 204 - 246 °C
399 - 475 °F
Typical