IRPC Polimaxx Polene 2500PC Polypropylene Block Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 2500PC Polypropylene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: MEDIUM FLOW, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS, ICE CREAM CUPS, CONTAINERS
Physical Properties Metric English Comments
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 87
87
ASTM D785
Tensile Strength, Yield 23.0 MPa
3340 psi
ASTM D638
Elongation at Yield 17 %
17 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
DIN 53453
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 190 - 240 °C
374 - 464 °F