Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 190 - 279 °C | 374 - 535 °F | Average value: 229 °C Grade Count:4 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Processing Temperature | 252 - 279 °C | 485 - 535 °F | Average value: 266 °C Grade Count:6 |
Overview of materials for Nylon 612 with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app.. |
|||
Processing Temperature | 252 - 279 °C | 485 - 535 °F | Average value: 266 °C Grade Count:17 |
Overview of materials for Nylon 612, Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of.. |