Processing Properties Metric English Comments
Processing Temperature 250 - 330 °C
482 - 626 °F
PolyChem Alloy PolyFoam 4004HF
PolyFoam decomposes when heated to create a uniform microcellular structure. It can be used in extrusion and injection molding processes to reduce weight in parts without adversely affecting the ph..
Processing Temperature 230 - 330 °C
446 - 626 °F
Average value: 283 °C Grade Count:15
Overview of materials for EMAAA Terpolymer
This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M..
Processing Temperature 288 - 330 °C
550 - 626 °F
Average value: 328 °C Grade Count:31
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Processing Temperature 288 - 330 °C
550 - 626 °F
Average value: 328 °C Grade Count:24
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Carbon Fiber Filler". Specific grades with carbon fiberr content be..
Processing Temperature 288 - 330 °C
550 - 626 °F
Average value: 321 °C Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max..
Processing Temperature 140 - 330 °C
284 - 626 °F
Average value: 300 °C Grade Count:11
Overview of materials for Polyphenylene Sulfide (PPS), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Aramid Fiber". Each property range of values reported is minimum and maximu..
Processing Temperature 221 - 330 °C
430 - 626 °F
Average value: 276 °C Grade Count:19
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Processing Temperature 320 - 330 °C
608 - 626 °F
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Processing Temperature 320 - 330 °C
608 - 626 °F
Eurotec® Tecomid® NT40 GR30 NL XA60 PPA, 30% glass fiber reinforced, flame retardant - halogen & red phosphorus free, heat stabilized, natural
Information provided by Eurotec®
Processing Temperature 270 - 330 °C
518 - 626 °F
E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate
10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
Processing Temperature 270 - 330 °C
518 - 626 °F
E-Polymers TEKANATE™ G715FR , Flame Retardant, 15% Glass Fiber Reinforced Poly Carbonate
15% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Processing Temperature 270 - 330 °C
518 - 626 °F
E-Polymers TEKANATE™ G720 , 20% Glass Fiber Reinforced Poly Carbonate
20% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
Processing Temperature 270 - 330 °C
518 - 626 °F
E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate
30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
Processing Temperature 270 - 330 °C
518 - 626 °F
E-Polymers TEKANATE™ G730FR , Flame Retardant, 30% Glass Fiber Reinforced Poly Carbonate
30% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd.
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi..
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® 3410 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3410 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3410 is a versatile adhesive for extrusion coating or lam..
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® 3430 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3430 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 3430 is a versatile adhesive for extrusion coating or lam..
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lam..
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® 4403 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4403 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER 4403 is a versatile adhesive for extrusion lamination, de..
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des..
Processing Temperature 270 - 330 °C
518 - 626 °F
Arkema Group LOTADER® TX 8030 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER TX 8030 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high pressure autoclave process. LOTADER TX 8030 is an adhesive designed for extrusion coating ..
Processing Temperature 296 - 330 °C
565 - 626 °F
Average value: 318 °C Grade Count:17
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled