Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKANATE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 83.0 MPa
12000 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D638
Flexural Yield Strength 125 MPa
18100 psi
ASTM D790
Flexural Modulus 3.50 GPa
508 ksi
ASTM D790
Izod Impact, Notched 0.950 J/cm
1.78 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 147 °C
297 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 143 °C
289 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Processing Temperature 270 - 330 °C
518 - 626 °F
Mold Temperature 90.0 - 110 °C
194 - 230 °F
Users viewing this material also viewed the following: