E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKANATE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 180 MPa
26100 psi
ASTM D790
Flexural Modulus 7.20 GPa
1040 ksi
ASTM D790
Izod Impact, Notched 1.50 J/cm
2.81 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 148 °C
298 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 147 °C
297 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Processing Temperature 270 - 330 °C
518 - 626 °F