Material Notes:
BMC 2400 is a general purpose BMC for applications in the field of low smoke density and non toxic smoke.. The flammability meets the demands of EN45545 and is classified according to British standard BS 6853 level 1 b. Certificates are available on request. The glass content is on a level that combines good mouldability with good mechanical properties regarding strength and stiffness.Information Provided by Menzolit
Physical Properties Metric English Comments
Water Absorption <= 0.50 %
<= 0.50 %
ISO 62
Mechanical Properties Metric English Comments
Elongation at Yield 0.00 %
0.00 %
tensile rupture strain; ISO 527-4
Poissons Ratio 0.30
0.30
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C
6.67 µin/in-°F
ISO 11359-2
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K
4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C
329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 150 °C
>= 302 °F
ISO 75-2
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 165 °C
329 °F
ISO 11357-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
IEC 60093
Comparative Tracking Index 600 V
600 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 135 - 150 °C
275 - 302 °F
Injection moulding, matched metal die