Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® M90AW POM, Tribological
(Unverified Data**) Celcon® M90AW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear in low load-high velocity applications. Celcon® M90AW is an option .. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 9021 S1 POM, Tribological
(Unverified Data**) modified with silicon oilInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological
(Unverified Data**) POM copolymerTribological, Low EmissionInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese VECTRA A515 LCP, 15% Mineral Reinforced
(Unverified Data**) Easier flow and slightly improved toughness over A530. Outstanding hydrolytic stability. 15% mineral filled.15% mineral filledA three-zone screw evenly divided into feed, compression, and metering.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese VECTRA E130i LCP, 30% Glass Reinforced
(Unverified Data**) High temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.30% glass fiber, e.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese VECTRA MT1310 LCP, 30% Medical Technology
(Unverified Data**) The Standard for the Industry. Excellent balance of properties, including easy flow, easy processing, thermal stability, chemical resistance, mechanical and electrical properties. Suitable for vapo.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese VECTRA S475 LCP, 32% Mineral / Glass Reinforced
(Unverified Data**) Super High Flow, High heat Resistance and Low Warp for Thin Parts.Super High Flow, High heat Resistance and Low Wrap for Thin PartsInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 150 °C | 176 - 302 °F | Hardening Temperature |
Möller Medical NanoSkin KL-VP NanoCoating Hard, scratch-resistant, brittle coating with resistance to high temperatures and chemicals, bioinert.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Processing Temperature | 80.0 °C | 176 °F | show side |
Lubrizol Telene 1610 A/B & A/BK Dicyclopentadiene (DCPD) Telene® is a two-component system based on extra-high purity dicyclopentadiene (DCPD). Telene® is processed using a standard high-pressure RIM Equipment (Reaction Injection Molding). Telene® resu.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® AM90S POM, Specialty Hostaform« acetal copolymer grade AM90S is a standard melt flow acetal copolymer grade containing an antimicrobial ingredient. Hostaform« AM90S provides the same physical and mechanical performan.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 2521 POM, Unfilled Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 9021 S1 POM, Tribological Information provided by Celanese |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultramid® A3EG10 50% Glass Filled PA66 (Dry) Description: 50% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness as well as for electric insulating parts.Information provided by BASF |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® MR130ACS POM, Specialty Hostaform« acetal copolymer grade MR130ACS is a general purpose acetal with improved acid stabilization. Hostaform« MR130ACS demonstrates improved performance over standard acetals after intermit.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese THERMX TE3002 PCT, 30% Glass Reinforced Thermx« TE3002 is a 30% glass fiber reinforced, flame retardant, black high performance polyester resin for injection molding.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA E130i LCP, 30% Glass Reinforced High temperature capability, easiest flow. Suitable where very thin walls are required. Used for broad range of SMT applications, with minimal dimensional change. 30% glass filled.Information provid.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese ZENITE 7130 LCP, 30% Glass Reinforced Zenite« 7130 is a 30% glass fiber reinforced liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.Information provided by Celan.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® MR25B POM, Specialty Celcon« MR25B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 100 °C | 176 - 212 °F | cavity |
Celanese Celstran® PA66-GF50-02 P11/14 Nylon 66, 50% Glass Reinforced Material code according to ISO 1043-1: PA66Information provided by Celanese |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultramid® A3HG6 HR BK 23591 30% Glass Filled PA66 (Dry) Description: 30% glass-fiber reinforced injection-molding grade with enhanced hydrolysis resistance, e.g., for applications in vehicle cooling systems.Information provided by BASF |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese ZENITE 17311 EFT LCP, 35% Mineral / Glass Reinforced ZENITE« 17311 EFT is a 35% glass and mineral reinforced grade. This grade offers excellent flowability, low warpage, excellent surface appearance, and excellent dimensional stability. Application f.. |
|||
Processing Temperature | 80.0 - 105 °C | 176 - 221 °F | Cavity temperature |
Celanese Hostaform® LX90 POM
(Unverified Data**) Preliminary Data Sheetgeneral pupose unfilled molded in metallic appearanceInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® S 9362 XAP² ™ POM, Impact Modified
(Unverified Data**) Preliminary Data SheetImpact modified, improved modulus and weld line, low emissionInformation provided by Celanese |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Dry) Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 36021 POM, Unfilled Hostaform« C 36021 is an unfilled acetal copolymer grade formulated for high flow while retaining a good balance of mechanical properties.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 105 °C | 176 - 221 °F | cavity |
Celanese Hostaform® LM140LG POM, Specialty Hostaform« acetal copolymer grade LM140LG is a laser markable specialty grade of acetal copolymer formulated to provide good flow with a low gloss finish.Information provided by Celanese |
|||
Processing Temperature | 80.0 °C | 176 °F | Hopper Throat |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA E830iPd LCP, 30% Specialty 30% glass filled Platable grade.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese ZENITE ZE55201 LCP, 50% Mineral / Glass Reinforced Zenite« ZE55201 is a 50% mineral/glass fiber reinforced liquid crystal polymer for injection molding. and It is specifically suitable for applications requiring ultra flatness.Information provided .. |