Material Notes:
Silver Ink C2010829D2 is a high definition silver ink for LTCC tape. It is compatible with other members of the GEM range of Silver LTCC Inks and most LTCC tape systems on the market.The ink has been made at a ready to use viscosity and should be thoroughly stirred before use avoiding introduction of air bubbles. It can be printed on automatic and semi automatic screen printers.Information provided by Gwent Electronic Materials Ltd.
Physical Properties Metric English Comments
Solids Content 79 - 81 %
79 - 81 %
Particle Size <= 4.0 µm
<= 4.0 µm
Main Break; Fineness of Grind
<= 12 µm
<= 12 µm
3rd Streak; Fineness of Grind
Viscosity 48000 cP

@Shear Rate 100 1/s,
Temperature 25.0 °C
48000 cP

@Shear Rate 100 1/s,
Temperature 77.0 °F
Haake VT550 cone and plate viscometer (PK1.1°)
Storage Temperature 20.0 °C
68.0 °F
Electrical Properties Metric English Comments
Surface Resistivity per Square 0.0025 ohm
0.0025 ohm
fired; 21 microns thick
Processing Properties Metric English Comments
Processing Temperature 120 - 150 °C
248 - 302 °F
Cure Time 10.0 - 15 min
0.167 - 0.25 hour
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Coverage cm2/g 95
230 mesh stainless steel screen
Printing Mesh counts/inch 180 to 340