Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation

Category Polymer , Thermoset , Silicone
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Versilic™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Versilicâ„¢ SPX-70I.B. High Strength Silicone Pressure Tubing Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Versilic™ SPX-70 I.B.: Produced form a proprietary combination of silicone elastomers, Versilic™ SPX-70 I.B. Tubing optimizes critical physical properties such as tensile strength, elongation and compression set, resulting in a more physically durable product. Its ultra-smooth inner bore reduces the risk of particle entrapment during fluid transfer. In addition, Versilic™ High-Strength Silicone Pressure Tubing will remain resilient and durable under extreme operating temperatures and repeated cleaning and sterilization. Versilic™ Silicone Tubing complies fully with the requirements of the USP Class VI Criteria and is entirely non-toxic, non-hemolytic and non-pyrogenic.Features/Benefits:Provides resiliency, long life and durabilityUltra-smooth inner bore reduces risk of particulate entrapmentTough braid reinforcement permits use under elevated working pressuresTaste and odor freeWithstands repeated CIP and SIP cleaning and sterilizationTemperature resistant from -112°F to 320°FMeets FDA, 3-A ad NSF criteriaTypical applications include Veterinary Pharmaceuticals, Sterile Filling and Processing, Water Purification Systems, Cosmetic Production, Beverage Dispensing, Food and Dairy Processing, High Temperature Chemical Processing, Sanitary Fitting Assembly.Information provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792-91
Water Absorption 0.080 %
0.080 %
24 hours at 23°C; ASTM D570-95
Mechanical Properties Metric English Comments
Hardness, Shore A 71
71
15 seconds; ASTM D2240-91
Tensile Strength, Yield 8.27 MPa
1200 psi
ASTM D412-92
Elongation at Break 300 %
300 %
ASTM D412-92
200% Modulus 0.00483 GPa
0.700 ksi
ASTM D412-92
Tear Strength 22.8 kN/m
130 pli
Initial Tear Strength; ASTM D624-91 Die B
Compression Set 10 %

@Temperature 70.0 °C
10 %

@Temperature 158 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
30 %

@Temperature 175 °C
30 %

@Temperature 347 °F
Constant Deflection, for 22 hrs.; ASTM D395-89 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Brittleness Temperature -80.0 °C
-112 °F
ASTM D746-95
Electrical Properties Metric English Comments
Dielectric Strength 20.1 kV/mm
511 kV/in
ASTM D149-93
Descriptive Properties Value Comments
Color Translucent