FeaturesChevron FM Greases EP are high performance, multipurpose food machinery greases that are white in color, odorless, tasteless, and water-resistant. Available in three grades, Chevron FM Greases EP were developed for the food processing and canning industries. Chevron FM Greases EP are a blend of a synthetic polyurea complex thickener and food grade white oils (Group II) containing a highly effective rust inhibitor. They are smooth and buttery in texture, and are slightly tacky.All grades contain a specially blended higher viscosity white mineral oil that imparts improved adhesive and stringiness properties to the grease.ApplicationsChevron FM Greases EP are multipurpose lubricants for all grease lubricated machinery in canneries, beverage bottlers and canners, potato/corn chip processors, candy manufacturers, meat and poultry packers, frozen food processors, and other food producers and processors. They are specifically recommended for critical applications where there is a possibility of the lubricant becoming an incidental or accidental food ingredient.NLGI 1 and 2 are preferred for general plant lubrication including applications such as electric motors and wheeled vehicles where USDA H2 lubricants are often used.NLGI 2 is also recommended for those applications where the grease is exposed to high temperatures, steam, and centrifugal action causing throw-off.
Physical Properties Metric English Comments
Viscosity Measurement 109
109
Viscosity Index; ASTM D2270
220
220
ISO viscosity grade
Saybolt Viscosity at 100°F 1060 SUS
1060 SUS
Saybolt Viscosity at 210°F 98 SUS
98 SUS
Kinematic Viscosity at 40°C (104°F) 202 cSt
202 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 19.4 cSt
19.4 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
Four Ball Wear 0.440 mm
0.0173 in
Penetration 280
280
worked
Penetration P(0), 1/10 mm 314
314
Timken Test 13600 g
30.0 lb
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Pour Point -13.0 °C
8.60 °F
ASTM D97
Flash Point 200 °C
392 °F
ASTM D92
Dropping Point 287 °C
549 °F
Descriptive Properties Value Comments
Color white
Lincoln Ventmeter, psig at 30 s, at 0°F 50
Lincoln Ventmeter, psig at 30 s, at -22°F too stiff at this temperature to pump through device
Lincoln Ventmeter, psig at 30 s, at 30°F 0
Lincoln Ventmeter, psig at 30 s, at 75°F 0
Texture smooth, buttery
Thickener, % / type 20.8 / Polyurea Complex