Polymer Property : Maximum Service Temperature, Air = 200 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 160 - 200 °C
320 - 392 °F
Parker Chomerics CHO-SEAL 1501 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Maximum Service Temperature, Air 130 - 200 °C
266 - 392 °F
Average value: 143 °C Grade Count:12
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Maximum Service Temperature, Air 120 - 200 °C
248 - 392 °F
Average value: 153 °C Grade Count:7
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Maximum Service Temperature, Air 170 - 200 °C
338 - 392 °F
Average value: 189 °C Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Maximum Service Temperature, Air 80.0 - 200 °C
176 - 392 °F
Average value: 140 °C Grade Count:10
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Maximum Service Temperature, Air 80.0 - 200 °C
176 - 392 °F
Average value: 124 °C Grade Count:8
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Maximum Service Temperature, Air 80.0 - 200 °C
176 - 392 °F
Average value: 128 °C Grade Count:4
Overview of materials for Nylon 66, MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri..
Maximum Service Temperature, Air -60.0 - 200 °C
-76.0 - 392 °F
SMAC BARRIER® Damping Material
SMAC BARRIER® is a new material developed by SMAC to complete the range of solutions for noise reduction into an aircraft. SMAC BARRIER® is an acoustic layer designed to reduce the transmissio..
Maximum Service Temperature, Air 150 - 200 °C
302 - 392 °F
Goodfellow Polyvinyl Fluoride (PVF) Film
A semi-crystalline, colorless, transparent-translucent fluoropolymer with excellent weathering resistance, good chemical resistance and low permeability to gases; it is very slow burning and has a v..
Maximum Service Temperature, Air 180 - 200 °C
356 - 392 °F
Average value: 189 °C Grade Count:9
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a..
Maximum Service Temperature, Air 180 - 200 °C
356 - 392 °F
Average value: 190 °C Grade Count:4
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Maximum Service Temperature, Air 80.0 - 200 °C
176 - 392 °F
Average value: 123 °C Grade Count:6
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..
Maximum Service Temperature, Air 75.0 - 200 °C
167 - 392 °F
Average value: 132 °C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Copyright © lookpolymers.com All Rights Reserved