Material Notes:
Product description: Grilon B 70 GFE 15 H is a impact modified, heat stabilized PA 6 injection molding grade with 15% glass fiber reinforcement. Grilon B 70 GFE 15 H has the following important properties: High impact resistanceHigh stiffnessGood flowabilityGood processability Application examples are functional parts in automotive, structural components for furniture applications and housings for power tool.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Water Absorption 7.0 %
7.0 %
ISO 62
Moisture Absorption 2.00 %
2.00 %
ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
0.0010 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
0.0070 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 70.0 MPa
10200 psi
conditioned; ISO 527-1/-2
120 MPa
17400 psi
dry; ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
dry; ISO 527-1/-2
10 %
10 %
conditioned; ISO 527-1/-2
Tensile Modulus 3.00 GPa
435 ksi
conditioned; ISO 527-1/-2
6.00 GPa
870 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 7.00 J/cm²
33.3 ft-lb/in²
dry; ISO 179/1eU
8.00 J/cm²
38.1 ft-lb/in²
conditioned; ISO 179/1eU
6.00 J/cm²

@Temperature 30.0 °C
28.6 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
7.00 J/cm²

@Temperature 30.0 °C
33.3 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
dry; ISO 179/1eA
2.00 J/cm²
9.52 ft-lb/in²
conditioned; ISO 179/1eA
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.700 J/cm²

@Temperature 30.0 °C
3.33 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
22.2 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 100 µm/m-°C
55.6 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 100 - 120 °C
212 - 248 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
ISO 75-1/-2
Deflection Temperature at 8.0 MPa 55.0 °C
131 °F
ISO 75-1/-2
Flammability, UL94 HB
HB
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+12 ohm-cm
1.00e+12 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Strength 32.0 kV/mm
813 kV/in
conditioned; IEC 60243-1
35.0 kV/mm
889 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Interior
Form Granules
Industry & Consumer goods Housewares
Mechanical Engineering
Power transmission
Sports & Leisure
Tools & Accessories
Processing Injection Molding
Special Characteristics High impact or impact modified