Material Notes:
Microwave Absorber Material. Elastomer microwave absorber is designed to offer wide band attenuation within operating frequencies of 500 MHz to 18 GHz. CHO-MUTE 9000 incorporates a high tech silicone polymer system that offers the benefit of wide band absorption and high permeability in a lightweight and flexible product form.Applications: CHO-MUTE 9000 is effective in many applications to eliminate EMI/EMC problems in, transmitters, transceivers, microcontrollers, microprocessors etc.Hand held electronics, wireless voice or data telecommunications, infotainment, testing equipment, PDAsMilitary electronics C3l, navigation, GPS, ruggedized computers, night visionAntenna performance, surface current reductionOffice and telecommunication infrastructure equipment, computing, switch gear, power amplifiers, routersInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.40 g/cc
3.40 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Tensile Strength at Break 3.45 MPa
500 psi
Elongation at Break >= 200 %
>= 200 %
Tear Strength 10.5 kN/m
59.9 pli
Thermal Properties Metric English Comments
Thermal Conductivity 0.560 W/m-K
3.89 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 160 °C
320 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+6 ohm-cm
>= 1.00e+6 ohm-cm
Surface Resistivity per Square >= 1.00e+6 ohm
>= 1.00e+6 ohm
Shielding Effectiveness -23.0 dB

@Thickness 1.57 mm,
Frequency 8.00e+9 Hz
-23.0 dB

@Thickness 0.0620 in,
Frequency 8.00e+9 Hz
Microwave Absorption
-21.0 dB

@Thickness 2.36 mm,
Frequency 6.00e+9 Hz
-21.0 dB

@Thickness 0.0930 in,
Frequency 6.00e+9 Hz
Microwave Absorption
-14.0 dB

@Thickness 1.57 mm,
Frequency 1.05e+10 Hz
-14.0 dB

@Thickness 0.0620 in,
Frequency 1.05e+10 Hz
Microwave Absorption
-13.0 dB

@Thickness 0.813 mm,
Frequency 1.05e+10 Hz
-13.0 dB

@Thickness 0.0320 in,
Frequency 1.05e+10 Hz
Microwave Absorption
-12.0 dB

@Thickness 3.17 mm,
Frequency 4.00e+9 Hz
-12.0 dB

@Thickness 0.125 in,
Frequency 4.00e+9 Hz
Microwave Absorption
-10.0 dB

@Thickness 1.57 mm,
Frequency 1.55e+10 Hz
-10.0 dB

@Thickness 0.0620 in,
Frequency 1.55e+10 Hz
Microwave Absorption
-7.00 dB

@Thickness 2.36 mm,
Frequency 1.05e+10 Hz
-7.00 dB

@Thickness 0.0930 in,
Frequency 1.05e+10 Hz
Microwave Absorption
-7.00 dB

@Thickness 0.813 mm,
Frequency 1.55e+10 Hz
-7.00 dB

@Thickness 0.0320 in,
Frequency 1.55e+10 Hz
Microwave Absorption
-7.00 dB

@Thickness 1.57 mm,
Frequency 5.00e+9 Hz
-7.00 dB

@Thickness 0.0620 in,
Frequency 5.00e+9 Hz
Microwave Absorption
-7.00 dB

@Thickness 1.57 mm,
Frequency 5.50e+9 Hz
-7.00 dB

@Thickness 0.0620 in,
Frequency 5.50e+9 Hz
Microwave Absorption
-7.00 dB

@Thickness 2.36 mm,
Frequency 1.55e+10 Hz
-7.00 dB

@Thickness 0.0930 in,
Frequency 1.55e+10 Hz
Microwave Absorption
-6.00 dB

@Thickness 3.17 mm,
Frequency 1.55e+10 Hz
-6.00 dB

@Thickness 0.125 in,
Frequency 1.55e+10 Hz
Microwave Absorption
-5.00 dB

@Thickness 3.17 mm,
Frequency 5.50e+9 Hz
-5.00 dB

@Thickness 0.125 in,
Frequency 5.50e+9 Hz
Microwave Absorption
-5.00 dB

@Thickness 3.17 mm,
Frequency 1.05e+10 Hz
-5.00 dB

@Thickness 0.125 in,
Frequency 1.05e+10 Hz
Microwave Absorption
-5.00 dB

@Thickness 0.508 mm,
Frequency 1.05e+10 Hz
-5.00 dB

@Thickness 0.0200 in,
Frequency 1.05e+10 Hz
Microwave Absorption
-4.00 dB

@Thickness 0.508 mm,
Frequency 1.55e+10 Hz
-4.00 dB

@Thickness 0.0200 in,
Frequency 1.55e+10 Hz
Microwave Absorption
-3.00 dB

@Thickness 0.254 mm,
Frequency 1.55e+10 Hz
-3.00 dB

@Thickness 0.0100 in,
Frequency 1.55e+10 Hz
Microwave Absorption
-3.00 dB

@Thickness 0.508 mm,
Frequency 5.50e+9 Hz
-3.00 dB

@Thickness 0.0200 in,
Frequency 5.50e+9 Hz
Microwave Absorption
-3.00 dB

@Thickness 0.813 mm,
Frequency 5.50e+9 Hz
-3.00 dB

@Thickness 0.0320 in,
Frequency 5.50e+9 Hz
Microwave Absorption
-3.00 dB

@Thickness 2.36 mm,
Frequency 2.50e+9 Hz
-3.00 dB

@Thickness 0.0930 in,
Frequency 2.50e+9 Hz
Microwave Absorption
-3.00 dB

@Thickness 1.57 mm,
Frequency 2.50e+9 Hz
-3.00 dB

@Thickness 0.0620 in,
Frequency 2.50e+9 Hz
Microwave Absorption
-2.00 dB

@Thickness 0.254 mm,
Frequency 1.05e+10 Hz
-2.00 dB

@Thickness 0.0100 in,
Frequency 1.05e+10 Hz
Microwave Absorption
-1.00 dB

@Thickness 0.254 mm,
Frequency 5.50e+9 Hz
-1.00 dB

@Thickness 0.0100 in,
Frequency 5.50e+9 Hz
Microwave Absorption
0.00 dB

@Thickness 0.254 mm,
Frequency 5.00e+8 Hz
0.00 dB

@Thickness 0.0100 in,
Frequency 5.00e+8 Hz
Microwave Absorption
0.00 dB

@Thickness 0.508 mm,
Frequency 5.00e+8 Hz
0.00 dB

@Thickness 0.0200 in,
Frequency 5.00e+8 Hz
Microwave Absorption
0.00 dB

@Thickness 0.813 mm,
Frequency 5.00e+8 Hz
0.00 dB

@Thickness 0.0320 in,
Frequency 5.00e+8 Hz
Microwave Absorption
0.00 dB

@Thickness 1.57 mm,
Frequency 5.00e+8 Hz
0.00 dB

@Thickness 0.0620 in,
Frequency 5.00e+8 Hz
Microwave Absorption
0.00 dB

@Thickness 2.36 mm,
Frequency 5.00e+8 Hz
0.00 dB

@Thickness 0.0930 in,
Frequency 5.00e+8 Hz
Microwave Absorption
0.00 dB

@Thickness 3.17 mm,
Frequency 5.00e+8 Hz
0.00 dB

@Thickness 0.125 in,
Frequency 5.00e+8 Hz
Microwave Absorption
Descriptive Properties Value Comments
Composition Ferrous filled silicone