Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristics for its entire lifetime.Special Properties:• Excellent slide properties• Wear-resistant, even in abrasive applications• High mechanical strength• Self-lubricating• Vibration-free running• Low residual stress• Good lubricant resistance• High dynamic load-bearing capacity• Approved for use in the food industry (EU and FDA)Information provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 1.8 %

@Temperature 23.0 °C
1.8 %

@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 5.5 %

@Temperature 23.0 °C
5.5 %

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell M 82
82
dry; ISO 2039-2
Ball Indentation Hardness 140 MPa
20300 psi
dry; ISO 2039-1
Tensile Strength 80.0 MPa
11600 psi
ISO 527-1
Elongation at Break 50 %
50 %
ISO 527-1
Creep Strength 18.0 MPa

@Time 3.60e+6 sec
2610 psi

@Time 1000 hour
stress leading to 1% elongation; dry; ISO 899-1
Modulus of Elasticity 2.50 GPa
363 ksi
Compressive Yield Strength 22.0 MPa

@Strain 1.00 %
3190 psi

@Strain 1.00 %
dry; ISO 604
43.0 MPa

@Strain 2.00 %
6240 psi

@Strain 2.00 %
dry; ISO 604
79.0 MPa

@Strain 5.00 %
11500 psi

@Strain 5.00 %
dry; ISO 604
Charpy Impact Unnotched NB
NB
dry; ISO 179-1/1eU
Charpy Impact, Notched >= 0.500 J/cm²
>= 2.38 ft-lb/in²
dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.18
0.18
Sand Slurry 0.050
0.050
µm/km
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
90.0 µm/m-°C

@Temperature 23.0 - 100 °C
50.0 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
Melting Point 215 °C
419 °F
ISO 11357-1
Maximum Service Temperature, Air 90.0 °C

@Time 7.20e+7 sec
194 °F

@Time 20000 hour
105 °C

@Time 1.80e+7 sec
221 °F

@Time 5000 hour
160 °C

@Time <=86400 sec
320 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Glass Transition Temp, Tg 50.0 °C
122 °F
ISO 11357-1
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
dry; IEC 60093
Dielectric Constant 3.1

@Frequency 1.00e+6 Hz
3.1

@Frequency 1.00e+6 Hz
dry; IEC 60250
3.5

@Frequency 100 Hz
3.5

@Frequency 100 Hz
dry; IEC 60250
Dielectric Strength 22.0 kV/mm
559 kV/in
dry; IEC 60243-1
Dielectric Loss Index 0.015

@Frequency 100 Hz
0.015

@Frequency 100 Hz
dry; IEC 60250
0.016

@Frequency 1.00e+6 Hz
0.016

@Frequency 1.00e+6 Hz
dry; IEC 60250
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Color Blue