Material Notes:
Very stressed-relieved and high-molecular weight PA6.Temperature resistant from -40° to approx. 100°C and high stiffness, hardness and toughness. The good mechanical characteristics will be achieved only after conditioning, this material must be conditioned again after annealing.Properties:High strength and stiffnessHigh impact and notching impact strengthHigh heat deflection temperatureGood at dampeningGood glide and emergency operating featuresGood chemical stability against organic solvents and fuelsSize alteration by humidity absorption must be consideredDimension stability, electrical and mechanical properties may become affected by humidity absorptionApplications: Bearing parts (good sliding properties), gear wheels, pump parts, sliding rails, castors (reduction of the noise level), fittings
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ISO 1183
Water Absorption 6.5 %
6.5 %
ISO 62
Moisture Absorption at Equilibrium 2.2 %
2.2 %
ISO 62
Mechanical Properties Metric English Comments
Hardness, Shore D 83
83
ISO 868
Ball Indentation Hardness 165 MPa
23900 psi
ISO 209
Tensile Strength, Yield 80.0 MPa
11600 psi
ISO 527
Elongation at Break >= 50 %
>= 50 %
ISO 527
Modulus of Elasticity 3.47 GPa
503 ksi
ISO 527
Flexural Strength >= 100 MPa
>= 14500 psi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Thermal Conductivity 0.230 W/m-K
1.60 BTU-in/hr-ft²-°F
ISO 22007-4
Melting Point 220 °C
428 °F
DIN EN ISO 314
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 40.0 °C
104 °F
DIN EN ISO 3146
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
IEC 60093
Dielectric Constant 3.7

@Frequency 1.00e+6 Hz
3.7

@Frequency 1.00e+6 Hz
DIN 53483
Dielectric Loss Index 0.030

@Frequency 1.00e+6 Hz
0.030

@Frequency 1.00e+6 Hz
DIN 53483
Descriptive Properties Value Comments
Bondability yes
Color Natural
Physiological indifference according limited
FDA
yes
EEC