Dow SiLK™ I300 380 Semiconductor Dielectric Resin

Category Polymer
Manufacturer Dow Chemical
Trade Name SiLK™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow SiLK™ I300 380 Semiconductor Dielectric Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SiLK™ I300 380 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 380 is compatible with standard IC processing tools in todays fabrications. SiLK™ I300 380 is fluorine-free, thus is compatible with Ti and Ta barrier materials.Information provided by Dow
Physical Properties Metric English Comments
Water Absorption 0.24 %
0.24 %
80% R.H.
Thickness 0.380 microns
0.0150 mil
3000 rpm
0.330 - 0.465 microns
0.0130 - 0.0183 mil
2000-4000 rpm
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 89.0 MPa
12900 psi
Tensile Strength, Yield 60.0 MPa
8700 psi
Tensile Modulus 2.45 GPa
355 ksi
Thermal Properties Metric English Comments
CTE, linear 62.0 µm/m-°C

@Temperature 50.0 - 150 °C
34.4 µin/in-°F

@Temperature 122 - 302 °F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
0.230 W/m-K

@Temperature 125 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 257 °F
Glass Transition Temp, Tg >= 490 °C
>= 914 °F
Decomposition Temperature 450 °C
842 °F
1% weight loss per hour
Optical Properties Metric English Comments
Refractive Index 1.63
1.63
Electrical Properties Metric English Comments
Dielectric Constant 2.6

@Frequency 100000 Hz
2.6

@Frequency 100000 Hz
Dielectric Strength >= 400 kV/mm
>= 10200 kV/in