Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon TC600 Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Thermal Conductivity, Excellent Dielectric Constant Control and Phase Stability with TemperatureInformation provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 3.20 g/cc
0.116 lb/in³
Water Absorption 0.030 %
0.030 %
Outgassing - Total Mass Loss 0.00 %
0.00 %
Collected Volatile
0.020 %
0.020 %
Total Mass Loss
Mechanical Properties Metric English Comments
Peel Strength 1.40 kN/m
8.00 pli
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C
5.00 µin/in-°F
x direction
9.00 µm/m-°C
5.00 µin/in-°F
y direction
CTE, linear, Transverse to Flow 35.0 µm/m-°C
19.4 µin/in-°F
z direction
Thermal Conductivity 1.10 W/m-K
7.63 BTU-in/hr-ft²-°F
z
1.40 W/m-K
9.72 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 6.15

@Frequency 1.00e+10 Hz
6.15

@Frequency 1.00e+10 Hz
6.15

@Thickness 0.254 mm
6.15

@Thickness 0.0100 in
6.15

@Thickness 6.35 mm
6.15

@Thickness 0.250 in
Dissipation Factor 0.0020

@Frequency 1.00e+10 Hz
0.0020

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -75