Novum Glass Solid Soda-lime Uniform Series Glass Microspheres

Category Ceramic , Glass
Manufacturer Novum Glass LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Novum Glass Solid Soda-lime Uniform Series Glass Microspheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solid soda-lime glass microspheres in colorless powder form. Uniform Series Microspheres are used for controlling a bond line thickness in adhesive bonding. Solid glass microspheres are used in a variety of industries for maintaining a consistent space between objects, allowing for more repeatable results and fewer rejected parts. U-Series microspheres can be used for calibration where a NIST traceable size standard or identical particles are required. Information provided by Novum Glass, LLC.
Physical Properties Metric English Comments
Specific Gravity 2.40 - 2.60 g/cc
2.40 - 2.60 g/cc
Mechanical Properties Metric English Comments
Compressive Strength 276 MPa
40000 psi
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C

@Temperature 30.0 - 300 °C
5.00 µin/in-°F

@Temperature 86.0 - 572 °F
Softening Point 650 °C
1200 °F
Optical Properties Metric English Comments
Refractive Index 1.50 - 1.52
1.50 - 1.52
n<sub>D</sub>
Component Elements Properties Metric English Comments
Al2O3 0.0 - 5 %
0.0 - 5 %
CaO 6 - 15 %
6 - 15 %
Fe2O3 <= 1 %
<= 1 %
MgO 1 - 5 %
1 - 5 %
Na2O 10 - 20 %
10 - 20 %
SiO2 67 - 75 %
67 - 75 %