Thermal Properties Metric English Comments
CTE, linear 5.00 - 10.0 µm/m-°C

@Temperature 50.0 - 100 °C
2.78 - 5.56 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
CTE, linear 5.00 - 10.0 µm/m-°C

@Temperature 50.0 - 100 °C
2.78 - 5.56 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
CTE, linear 5.00 - 10.0 µm/m-°C

@Temperature 50.0 - 100 °C
2.78 - 5.56 µin/in-°F

@Temperature 122 - 212 °F
ISO 11359-2
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
CTE, linear 8.00 - 10.0 µm/m-°C
4.44 - 5.56 µin/in-°F
DIN 51045
Plansee Cu-MoCu-Cu Laminate
A high performance, three-layer composite.Characteristics:High thermal conductivityLow thermal expansionIdeal for heat dissipation applications related to: IGBT modules, RF packages, and LED chips, ..
CTE, linear 1.00 - 10.0 µm/m-°C
0.556 - 5.56 µin/in-°F
Average value: 5.67 µm/m-°C Grade Count:3
Overview of materials for Phenolic, Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values ..
CTE, linear 9.60 - 10.0 µm/m-°C

@Temperature 20.0 - 100 °C
5.33 - 5.56 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Cu/Mo/Cu 1:1:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 20.0 °C
4.44 - 5.56 µin/in-°F

@Temperature 68.0 °F
MMCC Al/B4C Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 20.0 °C
4.44 - 5.56 µin/in-°F

@Temperature 68.0 °F
MMCC Al/SiC Particulate Aluminum Matrix Composite
Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-309N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-309NM,Body Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-309T Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-322T Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-332N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 9.00 - 10.0 µm/m-°C

@Temperature 1000 °C
5.00 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CUN-B937 Nozzle Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories SSN-787N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories ZNS Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CSN-601N Plate Brick
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 50.0 - 150 °C
4.44 - 5.56 µin/in-°F

@Temperature 122 - 302 °F
IPC TM-650 2.4.41
Arlon AD1000 PTFE/Woven Fiberglass/Ceramic Filled Laminate for Microwave Printed Circuit Boards