Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-5 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-7 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-7B Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-8 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-8H Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-9 Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-9B Strontium Ferrite Ceramic Magnetic Material |
|||
CTE, linear | 9.00 - 9.50 µm/m-°C @Temperature 20.0 °C |
5.00 - 5.28 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance C-8B Strontium Ferrite Ceramic Magnetic Material |