Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 4.80 - 4.90 g/cc
0.173 - 0.177 lb/in³
Porosity 13 - 17 %
13 - 17 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.014715 GPa

@Temperature 1400 °C
<= 2.1343 ksi

@Temperature 2550 °F
Compressive Strength <= 147 MPa
<= 21300 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
ZrO2 93 - 96 %
93 - 96 %
Descriptive Properties Value Comments
Remarks For Ca added steel, Excellent Corrosion resistance