Chosun Refractories CSN-309NM,Body Plate Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Chosun Refractories
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chosun Refractories CSN-309NM,Body Plate Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.95 - 3.10 g/cc
0.107 - 0.112 lb/in³
Porosity 7.0 - 10 %
7.0 - 10 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.00981 GPa

@Temperature 1400 °C
<= 1.42 ksi

@Temperature 2550 °F
Compressive Strength <= 127 MPa
<= 18500 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 74 - 78 %
74 - 78 %
Carbon, C 7.0 - 9.0 %
7.0 - 9.0 %
ZrO2 6.0 - 8.0 %
6.0 - 8.0 %
Descriptive Properties Value Comments
Remarks Excellent resistance for Ca, Mn chemical attack, For Ca addition,high[Mn}and 0 steel