Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 3.15 - 3.30 g/cc
0.114 - 0.119 lb/in³
Porosity 5.0 - 7.0 %
5.0 - 7.0 %
Mechanical Properties Metric English Comments
Modulus of Rupture <= 0.014715 GPa

@Temperature 1400 °C
<= 2.1343 ksi

@Temperature 2550 °F
Compressive Strength <= 157 MPa
<= 22800 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
CTE, linear 8.00 - 10.0 µm/m-°C

@Temperature 1000 °C
4.44 - 5.56 µin/in-°F

@Temperature 1830 °F
Component Elements Properties Metric English Comments
Al2O3 80 - 85 %
80 - 85 %
Carbon, C 6.0 - 8.0 %
6.0 - 8.0 %
ZrO2 4.0 - 7.0 %
4.0 - 7.0 %
Descriptive Properties Value Comments
Remarks Strong resistance to thermal spalling, Excellent durability for corrosion