Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 - 282 °C
275 - 540 °F
Average value: 220 °C Grade Count:11
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
Deflection Temperature at 1.8 MPa (264 psi) 271 - 282 °C
520 - 540 °F
Average value: 277 °C Grade Count:4
Overview of materials for Polyamide-Imide, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Deflection Temperature at 1.8 MPa (264 psi) 165 - 282 °C
329 - 540 °F
Average value: 229 °C Grade Count:10
Overview of materials for Epoxy, Encapsulating, Glass or Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Glass or Mineral Filled". Each property range of values reported is minimum and ma..
Deflection Temperature at 1.8 MPa (264 psi) 200 - 282 °C
392 - 540 °F
Average value: 259 °C Grade Count:7
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Deflection Temperature at 1.8 MPa (264 psi) 170 - 282 °C
338 - 540 °F
Average value: 229 °C Grade Count:23
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Deflection Temperature at 1.8 MPa (264 psi) 155 - 282 °C
311 - 540 °F
Average value: 258 °C Grade Count:6
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..
Deflection Temperature at 1.8 MPa (264 psi) 260 - 282 °C
500 - 540 °F
Average value: 267 °C Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Deflection Temperature at 1.8 MPa (264 psi) 110 - 282 °C
230 - 540 °F
Average value: 237 °C Grade Count:35
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..