Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.54 - 1.80 g/cc
0.0556 - 0.0650 lb/in³
Average value: 1.72 g/cc Grade Count:19
Filler Content 50.0 %
50.0 %
Average value: 50.0 % Grade Count:4
Water Absorption 0.0100 - 0.0200 %
0.0100 - 0.0200 %
Average value: 0.0186 % Grade Count:7
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00214 cm/cm Grade Count:13
Linear Mold Shrinkage, Transverse 0.00300 - 0.00850 cm/cm
0.00300 - 0.00850 in/in
Average value: 0.00512 cm/cm Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121 - 123
121 - 123
Average value: 123 Grade Count:6
Tensile Strength, Ultimate 36.5 - 200 MPa
5300 - 29000 psi
Average value: 147 MPa Grade Count:17
94.0 - 179.953 MPa

@Temperature -40.0 - 120 °C
13600 - 26100.0 psi

@Temperature -40.0 - 248 °F
Average value: 142 MPa Grade Count:3
Elongation at Break 0.400 - 2.20 %
0.400 - 2.20 %
Average value: 1.19 % Grade Count:17
0.950 - 0.950 %

@Temperature -40.0 - 4.44 °C
0.950 - 0.950 %

@Temperature -40.0 - 40.0 °F
Average value: 0.950 % Grade Count:2
Modulus of Elasticity 9.65 - 41.7 GPa
1400 - 6050 ksi
Average value: 18.4 GPa Grade Count:14
21.4427 - 21.4427 GPa

@Temperature -40.0 - -40.0 °C
3110.05 - 3110.05 ksi

@Temperature -40.0 - -40.0 °F
Average value: 21.4 GPa Grade Count:2
Flexural Yield Strength 57.9 - 343 MPa
8400 - 49700 psi
Average value: 229 MPa Grade Count:18
269.585 - 269.585 MPa

@Temperature -40.0 - -40.0 °C
39100.1 - 39100.1 psi

@Temperature -40.0 - -40.0 °F
Average value: 270 MPa Grade Count:2
Flexural Modulus 10.3 - 39.2 GPa
1500 - 5690 ksi
Average value: 16.3 GPa Grade Count:19
9.55 - 18.6848 GPa

@Temperature -40.0 - 120 °C
1390 - 2710.04 ksi

@Temperature -40.0 - 248 °F
Average value: 15.7 GPa Grade Count:3
Izod Impact, Notched 0.641 - 3.68 J/cm
1.20 - 6.90 ft-lb/in
Average value: 1.76 J/cm Grade Count:14
0.700 - 3.7373 J/cm

@Temperature -40.0 - -20.0 °C
1.31 - 7.0015 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 2.22 J/cm Grade Count:3
Izod Impact, Unnotched 3.20 - 5.34 J/cm
6.00 - 10.0 ft-lb/in
Average value: 3.83 J/cm Grade Count:6
Charpy Impact Unnotched 1.20 - 4.00 J/cm²
5.71 - 19.0 ft-lb/in²
Average value: 2.33 J/cm² Grade Count:3
1.20 - 1.20 J/cm²

@Temperature -40.0 - -20.0 °C
5.71 - 5.71 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 1.20 J/cm² Grade Count:1
Charpy Impact, Notched 0.600 - 2.80 J/cm²
2.86 - 13.3 ft-lb/in²
Average value: 1.49 J/cm² Grade Count:5
Thermal Properties Metric English Comments
CTE, linear 7.00 - 25.0 µm/m-°C
3.89 - 13.9 µin/in-°F
Average value: 15.7 µm/m-°C Grade Count:3
Melting Point 280 - 282 °C
536 - 540 °F
Average value: 281 °C Grade Count:3
Deflection Temperature at 0.46 MPa (66 psi) 266 - 280 °C
510 - 536 °F
Average value: 270 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 260 - 282 °C
500 - 540 °F
Average value: 267 °C Grade Count:17
Flammability, UL94 V-0
V-0
Grade Count:12
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 - 2.00e+16 ohm-cm
1.00e+15 - 2.00e+16 ohm-cm
Average value: 1.01e+16 ohm-cm Grade Count:7
Dielectric Constant 3.80 - 5.00
3.80 - 5.00
Average value: 4.18 Grade Count:3
Dielectric Strength 12.0 - 16.0 kV/mm
305 - 406 kV/in
Average value: 13.7 kV/mm Grade Count:3
Dissipation Factor 0.00100 - 0.00500
0.00100 - 0.00500
Average value: 0.00227 Grade Count:3
Comparative Tracking Index 125 - 175 V
125 - 175 V
Average value: 155 V Grade Count:3
Processing Properties Metric English Comments
Processing Temperature 70.0 - 340 °C
158 - 644 °F
Average value: 233 °C Grade Count:9
Die Temperature 290 - 345 °C
554 - 653 °F
Average value: 312 °C Grade Count:5
Melt Temperature 20.0 - 345 °C
68.0 - 653 °F
Average value: 286 °C Grade Count:11
Mold Temperature 130 - 177 °C
266 - 350 °F
Average value: 149 °C Grade Count:11
Drying Temperature 130 - 149 °C
266 - 300 °F
Average value: 138 °C Grade Count:8
Moisture Content 0.0200 - 0.0400 %
0.0200 - 0.0400 %
Average value: 0.0257 % Grade Count:7
Injection Pressure 50.0 - 103 MPa
7250 - 15000 psi
Average value: 82.5 MPa Grade Count:9
Users viewing this material also viewed the following: