Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 - 383 °C | 520 - 721 °F | Average value: 337 °C Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Annealed; ASTM D648 |
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ASTM D648 |
Quadrant EPP Duratron® PAI T5530 Compression Molded Glass Reinforced Polyamide-imide (ASTM Product Data Sheet) |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 - 280 °C | 520 - 536 °F | Average value: 278 °C Grade Count:6 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 - 282 °C | 520 - 540 °F | Average value: 277 °C Grade Count:4 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ISO 75 |
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontinued **)< Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ISO 75 |
Premix Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC
(discontin Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ASTM D648 |
PolyOne Edgetek® SF-40GF-25MN1/000 PPS (Polyphenylene Sulfide), 40% Glass Fiber and 25% Mineral Filled
(disco Information provided by PolyOne™ Corporation |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS GF/M65 BK 65% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 65% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS GF40 TL13 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS GF/M55 BK 55% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 55% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PPS/F GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ASTM D648 |
Plenco 08218 Polyester BMC, Compression Molded PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ASTM D648 |
Premix Premi-Glas® 1282-32 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1282-32 VE SMC is an enhanced high strength glass reinforced vinyl ester molding compound formulated for under-the-hood automotive applications.
Key features and benefi.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 271 °C | 520 °F | ASTM D648 |
Premix Premi-Glas® 1281-32 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1281-32 VE SMC is a high strength glass reinforced vinyl ester sheet molding compound formulated for under-the-hood automotive applications. Key features and benefits: Desi.. |