Thermal Properties Metric English Comments
Glow Wire Test 675 - 960 °C
1250 - 1760 °F
Average value: 820 °C Grade Count:6
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 783 °C Grade Count:6
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Glow Wire Test 725 - 960 °C
1340 - 1760 °F
Average value: 816 °C Grade Count:4
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Glow Wire Test 775 - 960 °C
1430 - 1760 °F
Average value: 868 °C Grade Count:8
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..
Glow Wire Test 850 - 960 °C
1560 - 1760 °F
Average value: 919 °C Grade Count:8
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 746 °C Grade Count:52
Overview of materials for Polypropylene with 20% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are ..
Glow Wire Test 390 - 960 °C
734 - 1760 °F
Average value: 685 °C Grade Count:19
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 871 °C Grade Count:8
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 865 °C Grade Count:7
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 871 °C Grade Count:3
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Glow Wire Test 649 - 960 °C
1200 - 1760 °F
Average value: 762 °C Grade Count:10
Overview of materials for Nylon 66, 30% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are inclu..
Glow Wire Test 825 - 960 °C
1520 - 1760 °F
IEC 60695-2-13
SABIC Innovative Plastics LNP LUBRICOMP OFL38A PPS - Branched (Europe-Africa-Middle East)
LNP* LUBRICOMP* OFL38A is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features include : Internally Lubricated.
Glow Wire Test 875 - 960 °C
1610 - 1760 °F
IEC 60695-2-13
SABIC Innovative Plastics LNP LUBRICOMP OFL38A PPS - Branched (Europe-Africa-Middle East)
LNP* LUBRICOMP* OFL38A is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features include : Internally Lubricated.
Glow Wire Test 775 - 960 °C
1430 - 1760 °F
Average value: 866 °C Grade Count:3
Overview of materials for Polyvinyl Dichloride (PVDC)
This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 869 °C Grade Count:11
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 857 °C Grade Count:3
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 753 °C Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Glow Wire Test 750 - 960 °C
1380 - 1760 °F
Average value: 915 °C Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% ..
Glow Wire Test 650 - 960 °C
1200 - 1760 °F
Average value: 903 °C Grade Count:13